The procurement of central pole lights focuses on six points: material, wall thickness, diameter, weld seam, galvanizing, and spray coating. The central pole lamp of clear thinking meets all these requirements.


中杆灯采购

这六个点不注意肯定踩坑


快速回答:

     中杆灯采购盯住六个点:看材质、看壁厚、看口径、看焊缝、看镀锌、看喷塑。明思维的中杆灯,这些要求全部达标。



01

 一个真实的教训:只看价格,装上去三个月就出问题

     我们明思维接待过一个和别家签合同单的客户,客户签的合同单里:中杆灯,壁厚未明确标注,口径未明确标注,锌层没标注,焊缝没要求,灯盘焊接要求也没提,只给了一个高度。


     客户当时图便宜,装上去三个月,杆子晃得厉害,焊缝还裂了,灯盘上的灯具也跟着晃。现在回来问怎么办。


     中杆灯采购,只看价格不看参数,装上去就后悔,好在他后来找到了我们明思维,同样是中杆灯,我们明思维是怎么做的?盯住六个点!




02

 中杆灯采购,盯住六个点




第一,看材质


常规要求一般采用Q235-B 材料(常规路灯一般都会选用Q235-B的材料),要求高的采用Q355-B / Q420-B / Q460-B,如果是低温极寒地区,采用-C / -D材料。




第二,看壁厚


中杆灯高度15到18米,壁厚必须符合杆体结构强度需求才能保证结构稳固。

壁厚不够,大风天一吹就会出现弯曲、断裂的现象。




第三,看口径

中杆灯高度15到18米,口径必须符合杆体抗风要求才能保证结构稳固。

口径不够,大风天一吹就弯。




第四,看焊缝

所有的焊接部位,焊缝必须饱满、无气孔、无咬边、无漏焊,要符合对应探伤要求。




第五,看镀锌

锌层厚度要大于86μm,才能保证户外长期不生锈。非热浸锌产品,或者是热浸锌不达标产品,两三年就会开始生锈,严重影响使用寿命和产品结构安全。



第六,看喷塑

塑粉要满足耐候性、抗紫外线、耐盐雾、附着力、塑粉流平性、遮盖力、高光粉的光泽度,同时还要关注杆体打磨处理的情况。烘烤温度和烘烤时间也一定要把握好。



03

 明思维的中杆灯,这些要求全部达标


     明思维交通照明的中杆灯,从材质选型、壁厚口径核算,到焊缝探伤、热镀锌、静电喷塑,每一道工序都按标准执行。

     是不是真材实料,拿到产品就知道,产品是不会骗人的。





Q&A


Q1:中杆灯高度一般是多少?

A:中杆灯高度通常为15到18米,介于普通路灯(6-12米)和高杆灯(15-45米)之间,适用于城市道路、广场、工业园区等中等面积照明场景。



Q2:中杆灯材质怎么选?


A:常规要求采用Q235-B;要求高的采用Q355-B / Q420-B / Q460-B;低温极寒地区采用-C / -D材料。



Q3:中杆灯锌层厚度要求是多少?
A:锌层厚度要大于86μm,才能保证户外长期不生锈。非热浸锌产品或热浸锌不达标产品,两三年就会开始生锈。